| 1. Place
Master Lap on platen. Do not turn on power.
2. Drip a small amount of water around
the lap.
3. Remove one Ultralap from the
package and place it, shiny side down, on the Master Lap. The water
between the Ultralap and Master Lap should form enough of a seal to keep the Ultralap from
wrinkling during use. Remember - the oxide polish is on
the dull side of the Ultralap.
4. Screw down the laps.
5. Turn on machine and drip water on
the Ultralap during polishing. You will need to experiment to see what the correct
amount of drip is for your polishing. Some faceters find it better to use a lot of
water, others prefer less drip.
6. Use light - medium pressure on the
lap.
7. HAVE FUN!
With correct use of Ultralaps, you
should be able to polish between 2 - 7 stones per lap. |